Shanghai Moopec Ltd
                                                                                                           
Verified Supplier
8 Years
Since 2018
Menu

Customized CRNGO Steel Electrical Silicon Transformer Steel Sheet

Price Negotiable
Price: $1.5/kg ; $1450/Ton
MOQ: 500kg
Delivery Time: 15-21 days
Brand: Baosteel
Product Description

The relationship between non-oriented silicon steel sheet and oriented silicon steel sheet:
1. Both are cold-rolled silicon steel, but the silicon content is different. The silicon content of cold-rolled non-oriented silicon steel sheet is 0.5%-3.0%, and the silicon content of cold-rolled oriented silicon steel sheet is above 3.0%.
2. Differences in production process and performance: non-oriented silicon steel sheet has relatively lower technological requirements than oriented silicon steel sheet.
3. Performance and use: Due to the different performance characteristics of the two, there are differences in the direction of use. The most important use of cold-rolled non-oriented silicon steel sheet is for the manufacture of generators, so it is also called cold-rolled motor silicon steel. The main purpose of cold-rolled oriented silicon steel strip is for transformer manufacturing, so it is also called cold-rolled transformer silicon steel.

 

Non-Oriented Electrical Steel is manufactured as to render magnetic properties almost uniform in any direction of the coil. Used mainly for medium and large rotating machines, and small transformers.
●Exhibits almost uniform and excellent magnetic properties in all directions of a steel sheet.
●Typical applications: motors, generators, audio transformers, reactors, magnet switches, ballasts, magnetic fields, and electromagnets for accelerators

 

Dimensional and Shape Tolerances
Nominal Thickness(mm) Nominal Width(mm) Flatness(%) Camber Within 2m
800~1000(0~+0.15) 0.20(±0.02) ≤2 ≤1.0
0.35(±0.03)
0.50,0.65(±0.04)
>1000(0~+0.15) 0.20(±0.02)
0.35,0.50(±0.03)
0.65(±0.04)

 

A SERIES
Types Nominal Thickness(mm) Theoretical density(kg/dm³) Max. Core Loss P15/50(w/kg) Min. InductionB50(T) Min. Lamination Factor(%)
B35A210 0.35 7.6 2.1 1.62 95
B35A230 7.6 2.3 1.62 95
B35A250 7.6 2.5 1.62 95
B35A270 7.65 2.7 1.62 95
B35A300 7.65 3 1.62 95
B35A360 7.65 3.6 1.63 95
B35A440 7.7 4.4 1.64 95
B35A550 7.75 5.5 1.64 95
B50A230 0.5 7.6 2.3 1.62 96
B50A250 7.6 2.5 1.62 96
B50A270 7.6 2.7 1.62 96
B50A290 7.6 2.9 1.62 96
B50A310 7.65 3.1 1.62 96
B50A350 7.65 3.5 1.62 96
B50A470 7.65 4 1.63 96
B50A600 7.7 4.7 1.64 96
B50A700 7.75 6 1.66 96
B50A800 7.8 7 1.7 96
B50A1000 7.8 8 1.7 96
B50A1300 7.8 8 1.7 96
B65A470 0.65 7.85 3.7 1.7 97
B65A600 7.65 4.7 1.7 97
B65A700 7.75 4.9 1.7 97
B65A800 7.75 8 1.7 97
B65A1000 7.8 10 1.7 97
B65A1300 7.85 13 1.7 97

 

AH SERIES
Types Nominal Thickness(mm) Theoretical density(kg/dm³) Max. Core Loss P15/50(w/kg) Min. InductionB50(T) Min. Lamination Factor(%)
B35AH230 0.35 7.65 2.3 1.66 95
B35AH250 7.65 2.5 1.67 95
B35AH300 7.7 3 1.69 95
B50AH300 0.5 7.65 3 1.67 96
B50AH350 7.7 3.5 1.7 96
B50AH470 7.75 4.7 1.72 96
B50AH600 7.75 6 1.72 96
B50AH800 7.8 8 1.74 96
B50AH1000 7.85 10 1.75 96
AR SERIES
B35AR300 0.35 7.8 2.3 1.66 95
B50AR300 0.5 7.75 2.5 1.67 95
B50AR350 7.8 3 1.69 95

Notes:                                                                                                                                              a. Test according to GB/T3655-2008.                                                                                                  b. The test specimen is half in both vertical and horizontal directions.                                                      c. The magnetic performance test of stress-relieving annealing high-efficiency non-oriented electrical steel AR series products is only applicable to the state of the sample after 2 hours of stress-relieving annealing at 750.
d. P15/50 means the core loss per kg sample when the maximum magnetic induction intensity is 1.5T and the frequency is 50Hz. P10/400 represents the core loss per kg sample when the maximum magnetic induction intensity is 1.0T and the frequency is 400Hz.                                                                       

e. B50 represents the magnetic induction intensity corresponding to the magnetic field intensity of 5000A/m.


 

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company Shanghai Moopec Ltd
Location Room 1808, Yibo Building, No. 10, Lane 1999, Wenchuan Road, Baoshan District, Shanghai 201901

Request A Quote

Please check your email address.
Your message must be at least 20 characters.