Product Description

Atomic Layer Deposition in Nanostructure and Pattern Industry
 
 
Applications

     Applications      Specific Purpose
     Nanostructure and pattern

     Template-assisted nanostructure

     Catalyst-assisted nanostructure
     Regioselective ALD for nanopattern preparation

 
Working Principle
Atomic layer deposition is a method of forming film by making the gaseous phase precursors pulsed alternately
into the reaction chamber and producing the gas-solid phase chemisorption reaction on the deposited substrate
surface. When the precursors reach the surface of the deposited substrate, they will be chemically adsorbed on
the surface and produce the surface reactions.

 
Features

     Model      ALD-NP-X—X
     Coating film system      AL2O3, TiO2, ZnO, etc
     Coating temperature range      Normal temperature to 500℃ (Customizable)
     Coating vacuum chamber size

     Inner diameter: 1200mm, Height: 500mm (Customizable)

     Vacuum chamber structure      According to customer’s requirements
     Background vacuum      <5×10-7mbar
     Coating thickness      ≥0.15nm
     Thickness control precision      ±0.1nm
     Coating size      200×200mm² / 400×400mm² / 1200×1200 mm², etc
     Film thickness uniformity      ≤±0.5%
     Precursor and carrier gas

     Trimethylaluminum, titanium tetrachloride, diethyl zinc, pure water,
     nitrogen, etc.

     Note: Customized production available.

                                                                                                                
Coating Samples

 

Process Steps
→ Place the substrate for coating into the vacuum chamber;
→ Vacuumize the vacuum chamber at high and low temperature, and rotate the substrate synchronously;
→ Start coating: the substrate is contacted with precursor in sequence and without simultaneous reaction;
→ Purge it with high-purity nitrogen gas after each reaction;
→ Stop rotating the substrate after the film thickness is up to standard and the operation of purging and cooling is

     completed, then take out the substrate after the vacuum breaking conditions are met.
 
Our Advantages
We are manufacturer.
Mature process.
Reply within 24 working hours.

 
Our ISO Certification

 

Parts Of Our Patents

 

Parts Of Our Awards and Qualifications of R&D


 
 
 
 
 
 
 
 
 
 

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company ZEIT Group
Location CSCES strait screen and core intelligent manufacturing base,Shuangliu District,Chengdu City, Sichuan Province, P. R. China
Contact Person Tyra

Request A Quote

Please check your email address.
Your message must be at least 20 characters.